1.1 This practice covers various types of cold rolled steel panels and the procedures to be followed in their preparation for testing paint, varnish, lacquer, conversion coatings, and related products.

1.2 The procedures are as follows: Procedure A -Conversion coatings (phosphates, chromates, etc.) Procedure B -Vapor degreasing Procedure C -Solvent brushing Procedure D -Solvent wiping Procedure E -Alkaline cleaning

1.3 This standard does not purport to address the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

(Back to all Standards)

 
   
Advertisements
 
Paint BidTracker

 
Sauereisen, Inc.

 
Strand’s Industrial Coatings

 
Tarps manufacturing, Inc.

 
Modern Safety Techniques

 
NLB Corporation

 
HoldTight Solutions Inc.

 
CRW

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us