B633 Standard Specification for Electrodeposited Coatings of Zinc on Iron and Steel

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: July 01, 2013
Updated On: July 10, 2013
Editorial Change:
 
This specification establishes the requirements for electrodeposited zinc coatings applied to iron or steel articles for corrosion protection purposes. Electrodeposited zinc-coated steel wires or sheets are not covered here. The coatings shall be provided in four standard thickness classes in the as-plated condition or with one of three types of supplementary finishes. The surfaces of the articles shall under go pre-plating basis metal cleaning, pre- and post-coating treatment for reducing the risk of hydrogen embrittlement, and reactivation and supplementary treatments. Coatings should be sampled, prepared, tested and conform accordingly to specified requirements as to appearance (luster and workmanship), thickness, adhesion, corrosion resistance, and hydrogen embrittlement.

This abstract is a brief summary of the referenced standard. It is informational only and not an official part of the standard; the full text of the standard itself must be referred to for its use and application. ASTM does not give any warranty express or implied or make any representation that the contents of this abstract are accurate, complete or up to date.

(Back to all Standards)

 
   

Tagged categories: Zinc
Advertisements
 
Axxiom Manufacturing

 
Tarps manufacturing, Inc.

 
CRW

 
Strand’s Industrial Coatings

 
EDCO - Equipment Development Co. Inc.

 
Sauereisen, Inc.

 
Abrasives Inc.

 
HoldTight Solutions Inc.

 
KTA-Tator, Inc. - Corporate Office

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us