D3624 Standard Test Method for Low Concentrations of Mercury in Paint by Atomic Absorption Spectroscopy

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: July 14, 2010
Updated On: July 22, 2010
Editorial Change:
 
The permissible level of heavy metals in certain coatings is specified by governmental regulatory agencies. This test method provides a fully documented procedure for determining low concentrations of mercury present in both water and solvent-reducible coatings to determine compliance.

This test method covers the determination of the content of mercury in the range between 10 and 1000 ppm (mg/kg) present in liquid coatings, coatings vehicles, or in dried films obtained from previously coated substrates. There is no reason to believe that higher levels could not be determined by this test method, provided that appropriate dilutions and adjustments in specimen size and reagent quantities are made.

(Back to all Standards)

 
   
Advertisements
 
HoldTight Solutions Inc.

 
CRW

 
Sauereisen, Inc.

 
Strand’s Industrial Coatings

 
Abrasives Inc.

 
Tarps manufacturing, Inc.

 
Axxiom Manufacturing

 
EDCO - Equipment Development Co. Inc.

 
KTA-Tator, Inc. - Corporate Office

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us