D5401 Standard Test Method for Evaluating Clear Water Repellent Coatings on Wood

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: March 16, 2009
Updated On: April 10, 2009
Editorial Change:
 
Water is known to penetrate wood substrates, causing dimensional instability and eventual deterioration. Clear water repellent coatings are designed to protect wood from damaging effects of water. This test method is used to evaluate the effectiveness of water repellent coatings on wood soon after application or after long-term exterior exposure.

1.1 This test method evaluates the effectiveness of clear water repellent coatings on wood before or after exterior exposure.

1.2 Intralaboratory results with this test method can be used to compare the effectiveness of clear water repellent coatings. The agreement between results obtained in different laboratories may be less satisfactory unless a known water repellent is used as a reference.

1.3 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.

1.4 This standard does not purport to address all of the safety problems, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

(Back to all Standards)

 
   
Advertisements
 
CRW

 
NLB Corporation

 
Sauereisen, Inc.

 
Paint BidTracker

 
Modern Safety Techniques

 
Strand’s Industrial Coatings

 
HoldTight Solutions Inc.

 
Tarps manufacturing, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us