A1055 Standard Specification for Zinc and Epoxy Dual-Coated Steel Reinforcing Bars

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: December 19, 2011
Updated On: January 16, 2012
Editorial Change:
 
This specification covers deformed and plain steel reinforcing bars with a dual coating of zinc alloy and an epoxy coating. The zinc alloy layer shall be applied by the thermal spray coating method followed by an epoxy coating, which shall be applied by the electrostatic spray method. The zinc coating shall conform to the required chemical composition for aluminum, cadmium, copper, iron, lead, tin, antimony, silver, bismuth, arsenic, nickel, magnesium, titanium, and zinc. The coated steel reinforcing bars shall conform to bend test requirements and to physical properties such as coating thickness, coating continuity, epoxy coating flexibility, and coating adhesion.

(Back to all Standards)

 
   
Advertisements
 
Strand’s Industrial Coatings

 
Paint BidTracker

 
CRW

 
HoldTight Solutions Inc.

 
NLB Corporation

 
Tarps manufacturing, Inc.

 
Modern Safety Techniques

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us