D4834 Standard Test Method for Detection of Lead in Paint by Direct Aspiration Atomic Absorption Spectroscopy

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: December 05, 2008
Editorial Change:
 
1.1 This test method is intended as a screening test to determine if the solids in a paint contain more than 0.06 % lead. The test described can differentiate between 0.05 and 0.06 %. Paints giving a result greater than 0.05 % should be analyzed quantitatively for lead using Test Method D 3335. This test method provides a more definitive and reliable screening test than Test Method D 3618.

1.2 There is no reason to believe that higher levels of lead could not be determined by this test method provided that appropriate dilutions and adjustments in specimen size and reagent quantities are made.

1.3 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

(Back to all Standards)

 
   
Advertisements
 
Modern Safety Techniques
 
Modern Safety Techniques
 
With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern
 

 
KTA-Tator, Inc. - Corporate Office
 
Instrument Service Department
 
Are you a QP certified contractor? KTA’s Instrument Service Department can help keep you compliant!
Click or call 1-800-KTA-GAGE.
 

 
Sky Climber, LLC
 
Solutions in Suspended Access
 
Safely reach workspaces regardless of size or purpose with our full line of Hoists, modular Platforms, and versatile Workcages.
 

 
BASF
 
New resins from BASF will have metals loving water!
 
Excellent corrosion resistance, low VOC, high gloss, thin films www.basf.us/industrialcoatings dpsolutions@basf.com 800-231-7868
 

 
ARC / A.W. Chesterton Company
 
Rapid Curing Coating
 
Cures under adverse conditions with maximum adhesion
 

 
NLB Corporation
 
NLB Sure Shroud: Greater Protection and Flexibility
 
NLB’s Sure Shroud’s lighter weight and flexibility reduces operator fatigue and offers unmatched protection against high pressure hose ruptures. 10k to 40k psi rated.
 

 
Novatek Corporation
 
Dustless Coatings Removal
 
Novatek Corporation, Dustless Coatings Removal Strip, clean and profile all dust free! Comply with new lead standards. Contact today: (866) 563-7800 www.Novatekco.com
 

 
Sauereisen, Inc.
 
Substrate Repair Materials
 

Substrate Repair Materials and Filler Compounds

Sauereisen's full line of underlayments are the ideal substrate repair materials to restore structural integrity prior to the application of SewerGard©
 

 
International Bridge Conference
 
Bridge conference 2018
 
Registration for the 2018 IBC is now open! Join us in June for the biggest and best IBC ever! View the Program, Workshops and Exhibitors by clicking in the banner.
 

 
HoldTight Solutions Inc.
 
Full Surface Protection for Up to One Year
 
HT 365 is a preservation, single component, anti-corrosive coating, a water displacing agent, a lubricant, and a penetrating fluid. It creates an imperceptible thin-film coating that offers excellent salt contaminant and humidity protection. Contact your HoldTight® representative or visit Holdtight.com for more information.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy (Updated 5/24/2018)   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us