1.1 This test method covers a procedure for determining the ability of a coating film and its substrate to resist shattering, cracking, or chipping when the film and substrate are distended beyond their original form by impact.

1.2 This test method does not measure impact resistance but uses rapid impact to improve Test Methods D 522, another test method for flexibility. Since the impact of the coating is almost instantaneous, all of the problems associated with time variables in the mandrel tests are eliminated.

1.3 This test method is similar in content but not technically equivalent to Test Method D 2794.

1.4 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

(Back to all Standards)

 
   
Advertisements
 
EDCO - Equipment Development Co. Inc.

 
Axxiom Manufacturing

 
KTA-Tator, Inc. - Corporate Office

 
CRW

 
HoldTight Solutions Inc.

 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
Abrasives Inc.

 
Strand’s Industrial Coatings

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us