G12 Standard Test Method for Nondestructive Measurement of Film Thickness of Pipeline Coatings on Steel

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: July 08, 2013
Updated On: July 10, 2013
Editorial Change:
 
3.1 Measurements of film thickness are an essential part of most ASTM test methods related to coatings on steel pipe. Adequate thickness is important for a coating to fulfill its function of preventing or mitigating corrosion of steel pipelines.

3.2 The accuracy of the thickness measurements may be influenced by the deformability of the coating. This test method is not applicable to coatings that would be readily deformable under the force exerted by the probe of the measuring instrument.



(Back to all Standards)

 
   
Advertisements
 
Fischer Technology Inc.
 
FISCHER Expands Corrosion Product Line
 
Rounding out Fischer’s extensive line of products for measuring protective coatings in the corrosion industry is the new ultrasonic wall thickness gauge UMP series.
 

 
KTA-Tator, Inc. - Corporate Office
 
KTA-TATOR LABORATORY SERVICES
 
• Coating failure analysis
• Independent testing
• Accelerated weathering testing
• Abrasives Testing
• Oil & Gas Material Qualification
• A2LA Certificate #2455.01
Contact: Rob Leggat
at 412-788-1300 x176
 

 
SAFE Systems, Inc.
 
Enduroguard -
The Tough Cable
for a Tough Industry.
 
Reduce maintenance costs and down time, increase job site safety with Enduroguard Cable. Available exclusively from SAFE Systems. UL listed, flexible, abrasion resistant and cut resistant.
 

 
ABKaelin, LLC
 
ABKAELIN EH&S SERVICES
 
Programs/Training/Monitoring for Silica, Lead, Noise, Beryllium, Hexavalent Chromium, Cadmium, Hazardous Waste*PM10 & TSP-Lead Ambient Air Monitoring*SSPC C3/C5
 

 
Blastox/The TDJ Group, Inc.
 
Blastox® - One Step Lead Abatement
 
Sandblast additive delivered to jobsite pre-blended to eliminate hazardous abrasive wastes. Why mix, meter or apply at the job-site? Blast with ease and
Let your painters paint!
1(800)-252-7869
 

 
International Bridge Conference
 
Bridge conference 2018
 
Registration for the 2018 IBC is now open! Join us in June for the biggest and best IBC ever! View the Program, Workshops and Exhibitors by clicking in the banner.
 

 
Tarps manufacturing, Inc.
 
QUALITY MADE IN AMERICA —Available near you!
 
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.
 

 
Carboline Company
 
Carboline launches new website!
 
The completely revamped website, offers quick and easy access to essential product information and is now mobile-friendly.
 

 
Graco Inc.
 
Graco EcoQuip 2: Experience the Difference
 
While others claim their equipment is the same, none of them compare to Graco’s EcoQuip 2™ Vapor Abrasive® blasting line. Visit graco.com/ecoquip to learn more.
 

 
ARC / A.W. Chesterton Company
 
Erosion Resistant Coating
 
It’s high gloss low drag, abrasion resistant surface extends equipment life, improves material flow, enhances equipment efficiency, and reduces downtime.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy (Updated 5/24/2018)   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us