F1330 Standard Guide for Metallic Abrasive Blasting to Descale the Interior of Pipe

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: January 24, 2007
Editorial Change:
 
1.1 This guide covers metallic abrasive blasting to descale the interior of carbon steel pipe.

1.2 This guide is recommended for use in conjunction with an abrasive reclamation system.

1.3 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.

This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

(Back to all Standards)

 
   
Advertisements
 
NLB Corporation

 
HoldTight Solutions Inc.

 
Strand’s Industrial Coatings

 
Sauereisen, Inc.

 
Modern Safety Techniques

 
Tarps manufacturing, Inc.

 
CRW

 
Paint BidTracker

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us