D478 Standard Specification for Zinc Yellow (Zinc Chromate) Pigments

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: November 14, 2006
Editorial Change:
 
1.1 This specification covers the pigments commercially known as zinc yellow (zinc chromate).

1.2 Two types are included: 1.2.1 Type I—High-purity, low sulfate and chloride content.

1.2.2 Type II—Regular grade.

1.3 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for informaiton only.

(Back to all Standards)

 
   
Advertisements
 
KTA-Tator, Inc. - Corporate Office

 
Fischer Technology Inc.

 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
SAFE Systems, Inc.

 
WEFTEC Show

 
DeFelsko Corporation

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us