D7232 Standard Test Method for Rapid Determination of the Nonvolatile Content of Coatings by Loss in Weight

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: August 02, 2012
Updated On: October 01, 2012
Editorial Change:
 
1.1 This test method is used to obtain rapid determination of the weight percent nonvolatile (solids) content via instrumental loss in weight technology. It is not meant as a replacement for Test Method D 2369.

1.2 This test method is principally intended for quality control labs and manufacturing environments where previously characterized materials will be tested repeatedly for different batches or lots.

1.3 This test method can be used for waterborne and solventborne resins, intermediates and finished paint products. This test method may not be applicable to all types of coatings.

1.4 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and to determine the applicability of regulatory limitations prior to use.

(Back to all Standards)

 
   
Advertisements
 
Paint BidTracker

 
Modern Safety Techniques

 
Strand’s Industrial Coatings

 
NLB Corporation

 
CRW

 
Sauereisen, Inc.

 
HoldTight Solutions Inc.

 
Tarps manufacturing, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us