A184 Standard Specification for Welded Deformed Steel Bar Mats for Concrete Reinforcement

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: November 10, 2011
Updated On: November 14, 2011
Editorial Change:
 
This specification covers the standard guide for welded deformed steel bar mats for concrete reinforcement. Mats should be capable of withstanding static load exerted perpendicular to the plane of the mat tending to separate the bars with no apparent loosening when applied to one intersection of the connected bars. Tension tests shall be performed on the specimen to determine the conformance to reference test materials. Also, test of connections against separation shall be performed on an assembled mat by placing blocks under a deformed bar in the upper layer and applying the prescribed load upon the bar in the lower layer.

1.1 This specification covers material in mat (or sheet) form fabricated from deformed steel bars to be used for the reinforcement of concrete. Mats consist of two layers of bars that are assembled at right angles to each other. Mats are assembled by welding at the intersections.

(Back to all Standards)

 
   
Advertisements
 
EDCO - Equipment Development Co. Inc.

 
Axxiom Manufacturing

 
Tarps manufacturing, Inc.

 
CRW

 
KTA-Tator, Inc. - Corporate Office

 
Sauereisen, Inc.

 
Abrasives Inc.

 
Strand’s Industrial Coatings

 
HoldTight Solutions Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us