1.1 This specification covers calcium chloride, technical grade, typically used for, but not limited to, dust control, stabilization, ice/snow removal, other road-conditioning purposes, acceleration of the set of concrete, and as a desiccant.

1.2 The values stated in SI units are to be regarded as the standard.

1.3 For purposes of determining conformance to this specification, values for chemical analysis shall be rounded to the nearest 0.1 %, and values for grading shall be rounded to the nearest 1 %, in accordance with the rounding method in Practice E 29.

1.4 The text of this standard references notes and footnotes, which provide explanatory material. These notes and footnotes (excluding those in tables and figures) shall not be considered as requirements of the standard.

(Back to all Standards)

 
   
Advertisements
 
KTA-Tator, Inc. - Corporate Office

 
EDCO - Equipment Development Co. Inc.

 
Sauereisen, Inc.

 
Abrasives Inc.

 
Axxiom Manufacturing

 
Strand’s Industrial Coatings

 
Tarps manufacturing, Inc.

 
HoldTight Solutions Inc.

 
CRW

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us