SSPC-TU 3, Overcoating

All Standards | SSPC Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: May 01, 1997
Updated On: April 01, 2002
Editorial Change: November 1, 2004
 
This technology update discusses the risks associated with the maintenance painting practice known as overcoating. Factors affecting overcoating application, service and costs are discussed.

This document is intended to serve as a resource for facility owners and others charged with developing and implementing maintenance painting programs.

Overcoating is one of several maintenance painting options. This document is not intended to provide a detailed description or comparison of the relative merit and cost considerations of overcoating versus other maintenance painting options. For a more complete and detailed discussion of maintenance painting practices, the reader should refer to SSPC-PA Guide 5, Guide to Maintenance Painting Programs.

(Back to all Standards)

 
   
Advertisements
 
Norton Sandblasting Equipment

 
Sauereisen, Inc.

 
Sherwin-Williams

 
Opta Waterdown, Inc.

 
NLB Corporation

 
Paint BidTracker

 
base painters

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us