D345 Standard Test Method for Sampling and Testing Calcium Chloride for Roads and Structural Applications

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: December 02, 2010
Updated On: February 02, 2011
Editorial Change:
 
This test method describes procedures to be used for sampling calcium chloride, and for determining grading of solid forms of calcium chloride for comparison with the requirements of a specification, such as Specification D98.

1.1 This test method covers sampling of solid and liquid forms of calcium chloride, and sieve analysis of solid form calcium chloride. Referee procedures for chemical analysis are covered in Test Methods E449.

1.2 A rapid method of chemical analysis is shown in Appendix X1. This rapid method is not to be used for determining chemical compliance of calcium chloride with specification requirements, such as in Specification D98.

1.1.1 This appendix covers a rapid method for chemical analysis of calcium chloride.

(Back to all Standards)

 
   
Advertisements
 
Modern Safety Techniques

 
Tarps manufacturing, Inc.

 
NLB Corporation

 
Strand’s Industrial Coatings

 
Sauereisen, Inc.

 
CRW

 
HoldTight Solutions Inc.

 
Paint BidTracker

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us