D235 Standard Specification for Mineral Spirits (Petroleum Spirits) (Hydrocarbon Dry Cleaning Solvent)

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: September 20, 2012
Updated On: October 01, 2012
Editorial Change:
 
1.1 This specification covers four types of hydrocarbon solvents, normally petroleum distillates, used primarily in the coatings and dry-cleaning industries. "Mineral spirits" is the most common name for these solvents. They are also called "Stoddard Solvents" when used for dry cleaning.

1.2 For specific hazard information and guidance, see the supplier's Material Safety Data Sheet for materials listed in this specification.

1.3 The following applies to all specified limits in this standard; for purposes of determining conformance with this standard, an observed value or a calculated value shall be rounded off "to the nearest unit" in the last right-hand digit used in expressing the specification limit, in accordance with the rounding-off method of Practice E 29.

1.4 The following hazard caveat pertains only to the test method portion, 6.1.10, of this specification.This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

(Back to all Standards)

 
   
Advertisements
 
SAFE Systems, Inc.

 
Modern Safety Techniques

 
Safety Lamp of Houston, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
RCG America

 
Norton Sandblasting Equipment

 
NLB Corporation

 
Sauereisen, Inc.

 
ABKaelin, LLC

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us