C140 Standard Test Methods for Sampling and Testing Concrete Masonry Units and Related Units

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: February 15, 2005
Editorial Change:
 
1.1 These test methods cover the sampling and testing of concrete masonry units for dimensions, compressive strength, absorption, unit weight (density), and moisture content. Flexural load testing and ballast weight determination of concrete roof pavers are also covered.

Note 1—The testing laboratory performing these test methods should be evaluated in accordance with Practice C 1093.

1.2 The values stated in inch-pound units are to be regarded as the standard. The values given in parentheses are for information only.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

(Back to all Standards)

 
   
Advertisements
 
Sauereisen, Inc.
 
Substrate Repair Materials
 

Substrate Repair Materials and Filler Compounds

Sauereisen's full line of underlayments are the ideal substrate repair materials to restore structural integrity prior to the application of SewerGard©
 

 
Norton Sandblasting Equipment
 
Norton Sandblasting Equipment
 
We are a premier stocking distributor for the leading manufacturers of surface preparation equipment, industrial dust collection, vacuums and more.
 

 
DeFelsko Corporation
 
PosiTector SHD Shore Hardness Durometer
 
PosiTector SHD measures the hardness of non-metallic materials. Features a measurement timer, auto ignore mode and internal memory. Shore A or D available.
 

 
HoldTight Solutions Inc.
 
Full Surface Protection for Up to One Year
 
HT 365 is a preservation, single component, anti-corrosive coating, a water displacing agent, a lubricant, and a penetrating fluid. It creates an imperceptible thin-film coating that offers excellent salt contaminant and humidity protection. Contact your HoldTight® representative or visit Holdtight.com for more information.
 

 
SAFE Systems, Inc.
 
Portable Blast &
Recovery Equipment
 
Trailer or skid mounted blast and recovery equipment. Systems designed for maximum versatility, environmental compliance
and overall cost savings.
Call 1-800-634-7278
 

 
KTA-Tator, Inc. - Corporate Office
 
New KTA Pipeline Inspection Kit
 
• Defelsko standard memory body
• Positector FTS 0-250 mils, cabled dry film thickness probe
• NEW Positector Shore D hardness probe
• All essential inspection equipment!
Visit www.ktagage.com
 

 
Novatek Corporation
 
Dustless Coatings Removal
 
Novatek Corporation, Dustless Coatings Removal Strip, clean and profile all dust free! Comply with new lead standards. Contact today: (866) 563-7800 www.Novatekco.com
 

 
Graco Inc.
 
Graco EcoQuip 2: Experience the Difference
 
While others claim their equipment is the same, none of them compare to Graco’s EcoQuip 2™ Vapor Abrasive® blasting line. Visit graco.com/ecoquip to learn more.
 

 
Modern Safety Techniques
 
Modern Safety Techniques
 
With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern
 

 
US Minerals
 
Blast with the best
 
The most effective blasting media on the market, Black Diamond hits harder and cleans faster.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us