This standard procedure describes a method for evaluating the qualification of shops whose primary function is surface preparation and coating application services. However, the procedure may be applicable to a fabricating shop, shipyard, or other entity that applies coatings in the shop, even though providing coating application services is not its primary function.

The procedure encompasses shop application of coatings in the industrial and light industrial/commercial market.

In addition to the evaluation criteria outlined in this procedure, the qualifying agency may elect to review the applicant's financial status and performance history in more detail than required by this procedure.

This standard is intended for work at fixed, permanent facilities. For field painting work that may involve the use of a temporary structure, evaluating contractors using Standard Procedure for Evaluating Painting Contractors (Field Application to Complex Industrial Structures), is more appropriate.

(Back to all Standards)

 
   
Advertisements
 
Norton Sandblasting Equipment

 
Axxiom Manufacturing

 
Opta Waterdown, Inc.

 
NLB Corporation

 
Sauereisen, Inc.

 
Tarps manufacturing, Inc.

 
Sherwin-Williams

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us