SSPC-PA Guide 4, Guide to Maintenance Repainting with Oil Base or Alkyd Painting Systems

All Standards | SSPC Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: November 01, 1982
Updated On: April 01, 2002
Editorial Change: November 1, 2004
 
This Guide covers the steps necessary for the repainting of steel structures previously painted with oil base, alkyd, or other conventional oleoresinous paint systems with the same generic paint system as the existing one.

(Back to all Standards)

 
   
Advertisements
 
Halifax Harbour Bridges

 
Nationwide Overspray

 
Thomas Industrial Coatings, Inc.

 
NLB Corporation

 
APV Engineered Coatings

 
base painters

 
Quikspray, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us