SSPC-Paint 38, Single-Component Moisture-Cure Weatherable Aliphatic Polyurethane Topcoat, Performance-Based

All Standards | SSPC Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: April 01, 2006
Updated On: May 18, 2004
Editorial Change:
 
This specification covers the requirements for a high performance single component moisture cure UV-stable polyurethane topcoat (ASTM D 16, Type II polyurethane). It is intended for a topcoat that provides good color and gloss retention.

Coatings meeting the requirements of this specification are generally suitable for exposures in environmental zones 1A (interior, normally dry), 1B (exterior, normally dry), 2A (frequently wet by fresh water, excluding immersion), 2B (frequently wet by salt water, excluding immersion), 3B (chemical exposure, neutral) and 3C (chemical exposure, alkaline).

The specified coating is intended for application by brush, spray, or roller. It is generally applied over a primer or intermediate coating.

(Back to all Standards)

 
   
Advertisements
 
Opta Waterdown, Inc.

 
Norton Sandblasting Equipment

 
Axxiom Manufacturing

 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
base painters

 
NLB Corporation

 
Paint BidTracker

 
Sherwin-Williams

 
Thomas Industrial Coatings, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us