INDUSTRIAL COATINGS QUIZ


Leaderboard: 12/24 - 1/23/2022
   Sign in to track your quiz score! |
Full Leaderboard

  • 1. Chuck Fite (19/19)

  • 2. michael beitzel (17/19)

  • 3. Mark Gierke (16/19)

  • 4. Juan I. Ordinas (14/19)

  • 5. Brian Dove (14/19)

  • 6. Bill Gradisher (14/19)

  • 7. Doug Driscoll, Sr. (14/19)

  • 8. Douglas Steitz (13/19)

  • 9. Pierpaolo Bonora (13/19)

  • 10. Haley Carnahan (12/19)

  • 11. Mark Anater (12/19)

  • 12. Yasuhiro Karakawa (12/19)

  • 13. Roland Peemans (12/19)

  • 14. Dave Heyne (11/19)

  • 15. Alex Hoogesteger (10/19)

  • 16. james hegarty (9/19)

  • 17. Jeff Rickert (7/19)

  • 18. Destiny Johnson (6/19)

  • 19. Greg Sutton (6/19)

  • 20. Paul Tsourous (6/19)


 

TUESDAY, AUGUST 27, 2019

What coating specialist said, “I don’t know how to calibrate a nose?”

Tom Aldinger
Mike O’Donoghue
Mark Schilling
Brian Goldie

Log in or register to PaintSquare save your results and track your cumulative quiz score!


Previous Quizzes from the Past Week

MONDAY, AUGUST 26, 2019
True or false: A mechanical rubbing machine is used to test a coating for solvent resistance.

FRIDAY, AUGUST 23, 2019
True or false: A three-year research study found that foul-release coatings were the most effective at combating macro-fouling organisms like zebra and quagga mussels.

THURSDAY, AUGUST 22, 2019
True or false: 3–6 mils is the typical range for the peak-to-valley height of surface profile created on steel by power-tool cleaning to bare metal and abrasive-blast cleaning.

WEDNESDAY, AUGUST 21, 2019
True or false: For spot repair of coatings, the selection of abrasive blasting as the surface preparation method is questionable.

TUESDAY, AUGUST 20, 2019
True or false: More than 60 organizations have sponsored content on PaintSquare.


More previous quizzes
Advertisements
 
Tarps manufacturing, Inc.

 
Strand’s Industrial Coatings

 
Modern Safety Techniques

 
CRW

 
HoldTight Solutions Inc.

 
NLB Corporation

 
Sauereisen, Inc.

 
Paint BidTracker

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us