INDUSTRIAL COATINGS QUIZ


Leaderboard: 3/2 - 4/1/2020
   Sign in to track your quiz score! |
Full Leaderboard

  • 1. Bryon Beck (23/23)

  • 2. Mark Gierke (23/23)

  • 3. Luis Ruiz (23/23)

  • 4. Juan I. Ordinas (22/23)

  • 5. Felipe Naciuk (22/23)

  • 6. Doug Driscoll, Sr. (22/23)

  • 7. Dirk Kuijken (21/23)

  • 8. Roland Peemans (21/23)

  • 9. Sid Stewart (21/23)

  • 10. Bill Gradisher (21/23)

  • 11. Brian Dove (20/23)

  • 12. Douglas Steitz (20/23)

  • 13. Robert Cloutier (20/23)

  • 14. Michael Beitzel (20/23)

  • 15. Dave Heyne (20/23)

  • 16. Mark Edmonds (19/23)

  • 17. Mark Allen (19/23)

  • 18. Lee Burke (18/23)

  • 19. Beau Ackx (18/23)

  • 20. Joe Doherty (17/23)


 

FRIDAY, MAY 10, 2019

Which of the following is used for in-service inspection of CUI systems?

Thermal imaging
Non-contact wall thickness sensors
Drones
All of these

Log in or register to PaintSquare save your results and track your cumulative quiz score!


Previous Quizzes from the Past Week

THURSDAY, MAY 9, 2019
The first U.S. patent describing abrasive blasting was issued in what year?

WEDNESDAY, MAY 8, 2019
True or false: A siloxepoxy is formed by the combination of epoxy with siloxane.

TUESDAY, MAY 7, 2019
True or false: In an air abrasive blasting system, the blast hose ID should be at least 3-4 times the size of the nozzle orifice to achieve productive blasting results.

MONDAY, MAY 6, 2019
True or false: Bimetallic corrosion, such as that which results when two dissimilar metals are connected electrically in a water tank interior, occurs most rapidly when the two metals are far apart rather than close together in the galvanic series.

FRIDAY, MAY 3, 2019
True or false: SSPC and NACE issue joint standards on abrasive blast cleaning, water and wet blast cleaning, cleaning of concrete and power tool cleaning.


More previous quizzes
Advertisements
 
DeFelsko Corporation

 
KTA-Tator, Inc. - Corporate Office

 
Sauereisen, Inc.

 
Tarps manufacturing, Inc.

 
SAFE Systems, Inc.

 
AWWA (American Water Works Association)

 
Fischer Technology Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us