COMMERCIAL COATINGS QUIZ


Leaderboard: 8/24 - 9/23/2020
   Sign in to track your quiz score! |
Full Leaderboard

  • 1. Mark Gierke (26/24)

  • 2. Phil Maguire (26/24)

  • 3. Luis Ruiz (24/24)

  • 4. Brandy Hadden (22/24)

  • 5. Bill Gradisher (21/24)

  • 6. Brian Dove (21/24)

  • 7. Radu Scurtescu (20/24)

  • 8. Roland Peemans (19/24)

  • 9. Ronald Syme (19/24)

  • 10. Bryon Beck (19/24)

  • 11. WH Seelinger (19/24)

  • 12. Yasuhiro Karakawa (18/24)

  • 13. Douglas Pearce (18/24)

  • 14. Dave Heyne (17/24)

  • 15. sachin chavhan (15/24)

  • 16. Marco Fabio Ramenzoni (15/24)

  • 17. Donald Molinari (13/24)

  • 18. Paul Bruni (12/24)

  • 19. Lance Mesngon (11/24)

  • 20. Harvey Brockman (11/24)


 

FRIDAY, DECEMBER 8, 2017

True or false: Solvent cleaning of steel is recommended to be used after other surface preparation methods such as abrasive blast cleaning.

True
False

Log in or register to PaintSquare save your results and track your cumulative quiz score!


Previous Quizzes from the Past Week

THURSDAY, DECEMBER 7, 2017
In abrasive blasting work, how small do dust particles have to be to make them respirable and therefore dangerous to health?

WEDNESDAY, DECEMBER 6, 2017
What term is used to describe the migration of asphalt from a roof to the surface of a white roof coating?

TUESDAY, DECEMBER 5, 2017
For high-heat applications (above 1,000 degrees Fahrenheit), organic zinc-rich coatings work best.

MONDAY, DECEMBER 4, 2017
What is the name of the analytical method that compares the composition of a particular batch of coating against a known standard for that coating?

FRIDAY, DECEMBER 1, 2017
True or false: Zinc coatings are sometimes applied to structural concrete to provide galvanic protection to the rebar.


More previous quizzes
Advertisements
 
Strategic Materials Inc.

 
KTA-Tator, Inc. - Corporate Office

 
WEFTEC Show

 
Sauereisen, Inc.

 
Tarps manufacturing, Inc.

 
SAFE Systems, Inc.

 
DeFelsko Corporation

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us