INDUSTRIAL COATINGS QUIZ


Leaderboard: 11/1 - 12/1/2021
   Sign in to track your quiz score! |
Full Leaderboard

  • 1. Mark Gierke (23/22)

  • 2. michael beitzel (22/22)

  • 3. Chuck Fite (22/22)

  • 4. Sid Stewart (21/22)

  • 5. Bill Gradisher (21/22)

  • 6. Dave Heyne (20/22)

  • 7. Douglas Steitz (20/22)

  • 8. Doug Driscoll, Sr. (20/22)

  • 9. Juan I. Ordinas (20/22)

  • 10. Brian Dove (20/22)

  • 11. mauricio gomez (19/22)

  • 12. Yasuhiro Karakawa (19/22)

  • 13. Pierpaolo Bonora (19/22)

  • 14. Roland Peemans (17/22)

  • 15. Alex Hoogesteger (15/22)

  • 16. Destiny Johnson (15/22)

  • 17. Jeff Rickert (14/22)

  • 18. Craig Anderson (14/22)

  • 19. Gus Dominguez (11/22)

  • 20. Marco Fabio Ramenzoni (10/22)


 

WEDNESDAY, JANUARY 25, 2017

Which of the following ISO 8501-1 standards is equivalent to SSPC-SP 6, Commercial Blast?

Sa1, Light Blast Cleaning
Sa2, Thorough Blast Cleaning
Sa21/2, Very Thorough Blast Cleaning
Sa3, Blast Clean to Visually Clean Steel

Log in or register to PaintSquare save your results and track your cumulative quiz score!


Previous Quizzes from the Past Week

TUESDAY, JANUARY 24, 2017
True or false: A discontinuity and a holiday both describe the same type of application error.

MONDAY, JANUARY 23, 2017
True or false: When a cold-weather coating is used to coat steel in temperatures below freezing, it is not necessary for the surface temperature of the steel to be at least 5 degrees Fahrenheit above the dew point temperature.

FRIDAY, JANUARY 20, 2017
What is it called when a coating controls corrosion by preventing the passage of soluble ions to the underlying steel?

THURSDAY, JANUARY 19, 2017
True or false: Wet film thickness gages are inadequate for measuring thickness of fast-set polyurea coatings.

WEDNESDAY, JANUARY 18, 2017
True or false: Use of a digital profile gage according to ASTM 4417-14 requires each area to receive 10 profile readings, and the highest measurement is recorded as the profile of the area being measured.


More previous quizzes
Advertisements
 
Abrasives Inc.

 
HoldTight Solutions Inc.

 
Sauereisen, Inc.

 
CRW

 
Strand’s Industrial Coatings

 
Axxiom Manufacturing

 
KTA-Tator, Inc. - Corporate Office

 
EDCO - Equipment Development Co. Inc.

 
Tarps manufacturing, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us