INDUSTRIAL COATINGS QUIZ


Leaderboard: 9/16 - 10/16/2021
   Sign in to track your quiz score! |
Full Leaderboard

  • 1. Douglas Steitz (24/26)

  • 2. Mark Gierke (23/26)

  • 3. Sid Stewart (22/26)

  • 4. Brian Dove (21/26)

  • 5. Pierpaolo Bonora (21/26)

  • 6. Juan I. Ordinas (21/26)

  • 7. Doug Driscoll, Sr. (21/26)

  • 8. michael beitzel (21/26)

  • 9. Chuck Fite (20/26)

  • 10. Destiny Johnson (20/26)

  • 11. Bill Gradisher (20/26)

  • 12. Dave Heyne (19/26)

  • 13. Yasuhiro Karakawa (19/26)

  • 14. Lee Burke (19/26)

  • 15. william farrell (18/26)

  • 16. blair Nixon,Jr. (17/26)

  • 17. Roland Peemans (16/26)

  • 18. Alex Hoogesteger (15/26)

  • 19. Mark Anater (13/26)

  • 20. Craig Anderson (13/26)


 

TUESDAY, JANUARY 24, 2017

True or false: A discontinuity and a holiday both describe the same type of application error.

True
False

Log in or register to PaintSquare save your results and track your cumulative quiz score!


Previous Quizzes from the Past Week

MONDAY, JANUARY 23, 2017
True or false: When a cold-weather coating is used to coat steel in temperatures below freezing, it is not necessary for the surface temperature of the steel to be at least 5 degrees Fahrenheit above the dew point temperature.

FRIDAY, JANUARY 20, 2017
What is it called when a coating controls corrosion by preventing the passage of soluble ions to the underlying steel?

THURSDAY, JANUARY 19, 2017
True or false: Wet film thickness gages are inadequate for measuring thickness of fast-set polyurea coatings.

WEDNESDAY, JANUARY 18, 2017
True or false: Use of a digital profile gage according to ASTM 4417-14 requires each area to receive 10 profile readings, and the highest measurement is recorded as the profile of the area being measured.

TUESDAY, JANUARY 17, 2017
True or false: According to a JPCL article on achieving peak performance from abrasives, the easiest way to adjust profile height in the field is by changing the velocity of the abrasive.


More previous quizzes
Advertisements
 
Axxiom Manufacturing

 
Sauereisen, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Tarps manufacturing, Inc.

 
CRW

 
Seal for Life/STOPAQ

 
Abrasives Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us