COMMERCIAL COATINGS QUIZ


Leaderboard: 8/19 - 9/18/2021
   Sign in to track your quiz score! |
Full Leaderboard

  • 1. Mark Gierke (25/25)

  • 2. Ronald Syme (23/25)

  • 3. Yasuhiro Karakawa (22/25)

  • 4. Brian Dove (20/25)

  • 5. Bill Gradisher (20/25)

  • 6. Phil Maguire (20/25)

  • 7. Roland Peemans (19/25)

  • 8. Chuck Fite (19/25)

  • 9. Douglas Pearce (18/25)

  • 10. Dave Heyne (17/25)

  • 11. Mark Anater (16/25)

  • 12. Pierpaolo Bonora (16/25)

  • 13. Destiny Johnson (15/25)

  • 14. Paul Tsourous (11/25)

  • 15. Phillip Harris (10/25)

  • 16. Jon Lawniczak (9/25)

  • 17. Perry Foreman (9/25)

  • 18. DrHeinzWilhelm Lange (8/25)

  • 19. mauricio gomez (8/25)

  • 20. Harvey Brockman (7/25)


 

WEDNESDAY, OCTOBER 29, 2014

True or false: The SSPC Committee on Commercial Coatings is developing guides for laboratory testing, selecting, and assuring the quality of thick-film coatings on CMU assemblies.

True
False

Log in or register to PaintSquare save your results and track your cumulative quiz score!


Previous Quizzes from the Past Week

TUESDAY, OCTOBER 28, 2014
What organization has studied, and reported on, the energy and moisture effects of EIFS?

MONDAY, OCTOBER 27, 2014
True or false: When dissimilar metals are in contact in the presence of an electrolyte, the more noble metal will experience galvanic corrosion.

FRIDAY, OCTOBER 24, 2014
True or false: SSPC has a qualification procedure (QP) to assure the qualifications of installers of liquid-applied air barriers.

THURSDAY, OCTOBER 23, 2014
True or false: The adhesion of coatings to weathered TPO roofing membranes can be significantly increased by using aqueous cleaners, followed by power washing.

WEDNESDAY, OCTOBER 22, 2014
True or false: Acrylic binders are sometimes used in intumescent coatings for building interiors.


More previous quizzes
Advertisements
 
Axxiom Manufacturing

 
KTA-Tator, Inc. - Corporate Office

 
Tarps manufacturing, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us