INDUSTRIAL COATINGS QUIZ


Leaderboard: 12/21 - 1/20/2022
   Sign in to track your quiz score! |
Full Leaderboard

  • 1. Mark Gierke (18/17)

  • 2. Chuck Fite (17/17)

  • 3. Douglas Steitz (17/17)

  • 4. michael beitzel (16/17)

  • 5. Doug Driscoll, Sr. (15/17)

  • 6. Juan I. Ordinas (15/17)

  • 7. Bill Gradisher (15/17)

  • 8. Brian Dove (14/17)

  • 9. Yasuhiro Karakawa (14/17)

  • 10. Roland Peemans (13/17)

  • 11. Alex Hoogesteger (12/17)

  • 12. Dave Heyne (12/17)

  • 13. Pierpaolo Bonora (12/17)

  • 14. Mark Anater (12/17)

  • 15. Haley Carnahan (11/17)

  • 16. james hegarty (9/17)

  • 17. Jeff Rickert (8/17)

  • 18. Paul Tsourous (7/17)

  • 19. L. Steven Moore (6/17)

  • 20. Greg Sutton (5/17)


 

TUESDAY, JANUARY 14, 2020

The “spreading rate of a coating to a completely flat surface, assuming no losses in handling” defines what term?

Aspirational coverage
Theoretical coverage
Desired coverage
None of these

Log in or register to PaintSquare save your results and track your cumulative quiz score!


Previous Quizzes from the Past Week

MONDAY, JANUARY 13, 2020
In dealing with coating thickness requirements, 25 microns equals approximately how many mils?

FRIDAY, JANUARY 10, 2020
True or false: In protective coatings, the rutile and not the anatase form of titanium dioxide is used.

THURSDAY, JANUARY 9, 2020
True or false: One-day results of relative humidity testing of concrete floors with in-situ probes is typically not accurate enough to judge if it is acceptable to apply materials that can tolerate higher moisture content.

WEDNESDAY, JANUARY 8, 2020
True or false: SSPC-SP 5, "White Metal Blast Cleaning," allows 5% of the blast-cleaned surface to have stains of old paint, rust or mill scale.

TUESDAY, JANUARY 7, 2020
What was the acronym for SSPC’s early research program on environmentally friendly coatings?


More previous quizzes
Advertisements
 
HoldTight Solutions Inc.

 
NLB Corporation

 
Modern Safety Techniques

 
CRW

 
Tarps manufacturing, Inc.

 
Paint BidTracker

 
Strand’s Industrial Coatings

 
Sauereisen, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us