I need to embed a metallized culvert liner on concrete. I've been told I have to paint it to avoid adhesion problems between the metal liner and the concrete. Is this true and, if so, what type of coating is best?
Selected Answers
From
Larry Muzia of Exceletech Coating & Applications, LLC on
May 28, 2020:
More information is needed to properly answer the ...read more
More information is needed to properly answer the question; however, it is very likely that a barrier coating may be required to prevent corrosion, assuming it is an aluminum or zinc metallizing.
From
Jaime Marcos of Profesional independiente on
May 26, 2020:
Clean the metallic surface and apply a layer of ad ...read more