What kind of coating system provides the strongest resistance to staining from hot tires on garage floors and parking decks?
Selected Answers
From
Carl Thompson of Hill Brothers on
May 3, 2011:
Two-part epoxy. ...read more
Two-part epoxy.
From
Daniel Reed of Delta Engineering on
April 28, 2011:
Sometimes the solution is the most simplistic. Con ...read more
Sometimes the solution is the most simplistic. Convince the customer that a black (or dark) concrete stain is the way to go as it will hide a certain amount of stains and dirt.