How clean must the compressed-air supply be for blast cleaning, blow down and painting? How is cleanliness of the air determined?
Selected Answers
From
Neil Pittman of Lake Superior Consulting on
May 14, 2020:
Clean to ASTM D4285 at the point of use, measured ...read more
Clean to ASTM D4285 at the point of use, measured each time the compressor is started or once per shift, whichever is more frequent.