Problem Solving Forum


February 24 - February 28, 2020

What are the pros and cons of using shotblasting to remove a coating system from a concrete floor?


Selected Answers

From john lienert of nehalem bay paint on February 28, 2020:
Expensive is a con. ...read more

Please sign in to submit your answer to this question
   

Tagged categories: Asia Pacific; EMEA (Europe, Middle East and Africa); Latin America; North America; Surface preparation; Surface Preparation