I keep reading references to sweep blasting, but I can't find a standard for it. What is sweep blasting, and is there a standard for it in the U.S. or elsewhere?


Selected Answers

From Jon Cavallo of Jon R. Cavallo PE LLC on February 22, 2020:
Don't forget about ISO 8501 Sa1, Light Blast-Clean ...read more

From Mark Edmonds of Placer Inspection on February 22, 2020:
Sweep blasting is a slang term used in the work pl ...read more

From Dong Duy of Alpha-ECC Vietnam on February 11, 2020:
SSPC-SP 7 for steel substrates and SSPC-SP 16 for ...read more