Problem Solving Forum


December 16 - December 20, 2019

What quality control checks can I use to assure the cleanliness of steel abrasive in a fabricator's or shipyard's shop?


Selected Answers

From sean newhall of NEWPORT FAB on January 4, 2020:
An oil/grease test is done with a clear jar of wat ...read more

From Toshihide Mori of Sasebo heavy industries, co.lud., on December 27, 2019:


Do a shipyard check prior to blasti ...read more

From Marco Fabio Ramenzoni of ZINGA METALL BRASIL on December 26, 2019:
Routine checking for the cleanliness of abrasives ...read more

From Gerard Apuzzi of Champion painting on December 25, 2019:
Conduct a tape test. ...read more

Please sign in to submit your answer to this question
   

Tagged categories: Abrasives; Quality Control