How much detail should be included in a specification for the surface preparation and painting of a parking garage exterior that includes tilt-up and structural concrete substrates?
Selected Answers
From
Sean Meracle of The Sherwin Williams Company on
May 20, 2019:
Aside from cleanliness, ICRI Guideline 310.2R-2013 ...read more
Aside from cleanliness, ICRI Guideline 310.2R-2013 is an excellent tool for communicating surface preparation expectations, utilizing the Concrete Surface Profile (CSP) comparators.