What is the best low-maintenance approach to coating power-tool-cleaned field weld joints on process pipework that is protected with thermal-sprayed aluminum?


Selected Answers

From Katheravan Arumugam of ENI on December 6, 2018:
I would suggest a suitable organic zinc rich with ...read more

From Bryant Chandler of Greenman-Pedersen, Inc. on November 27, 2018:
Going to the expense of applying TSA to the pipe, ...read more