When applying a 100% solids, fast-curing polyurea coating on concrete, what is the best method for verifying that the proper thickness has been applied?
Selected Answers
From
ROYER Jean baptiste of Protective Engineering on
January 25, 2018:
Stick a steel plate on concrete .
Define its rig ...read more
Stick a steel plate on concrete .
Define its right position on the structure.
After painting, you should be able to determine the thickness with a thickness gage.
From
Marc-André Vaillant of Dion Peinture industrielle on
January 16, 2018:
Calculate your flow rate by specific area and have ...read more