What type of material should I use to achieve bright, bold colors that will last on a concrete floor with heavy foot traffic?
Selected Answers
From
Jaime Molina of Primary Materials Inc. on
June 14, 2017:
A good option would be a metallic epoxy coat. This ...read more
A good option would be a metallic epoxy coat. This resin allows the installer to get as artistic with the colors as he or the architect wants. This surface can be topcoated with a good polyurea for an even more durable surface. Durable, artistic and not too expensive.
From
Zenith Czora of Durotech Industries, Inc. on
June 14, 2017:
You may use tintable, solvent-based acrylic sealer ...read more
You may use tintable, solvent-based acrylic sealer to be tinted to any color of your choice for your first and second coat, then topcoat with polyaspartic clear coating.
From
vijay shankar of level floorings on
June 13, 2017:
Broadcast dry-shake colored floor hardeners at a d ...read more
Broadcast dry-shake colored floor hardeners at a dosage of 5 kg per sq m on green concrete prior to floating and then polish the cured concrete surface to achieve excellent results.
From
chris atkins of mott macdonald on
June 12, 2017:
Stain the concrete, then use lighting. ...read more
Stain the concrete, then use lighting.