What type of coating system (and surface prep) should be used to protect a steel factory roof that is subject to hydrochloric acid vapors and other industrial pollutants and particulates in a hot, humid environment?


Selected Answers

From Antonio Moreno of INTERCHEM 2000 C.A. on May 17, 2017:
Novolac vinyl ester is the best option  for h ...read more

From William Slama of International Paint/Ceilcote Products on May 16, 2017:
Epoxy systems would not be a good choice for HCl v ...read more

From Per Gabrielsson of Free Lance Consultations and Inspections on May 15, 2017:
1500 um of glass-platelet-reinforced vinyl ester, ...read more

From Warren Brand of Chicago Corrosion Group on May 13, 2017:
We've worked on projects just like this in the pas ...read more

From Raymond Merrill of Texas Department of Transportation on May 9, 2017:
Ditto Mr. Neale. Is the factory roof a steel roof ...read more

From trevor neale of TF Warren Group on May 8, 2017:
Suggest more information is required. Is this for ...read more