What is the maximum temperature that an epoxy powder coating can resist when applied on steel substrate?
Selected Answers
From
Mustafa Dayyat of Sherwin-Williams Company - Performance Coatings Group on
November 22, 2016:
The temperature resistance and performance of epox ...read more
The temperature resistance and performance of epoxy powder coatings depends on the epoxy resin chemistry and the cross-linkers used to formulate the product.
From
Ajith Varghese of Internationalpaint on
November 21, 2016:
The maximum temperature an epoxy-based coating wit ...read more
The maximum temperature an epoxy-based coating withstands is between 100-120 C. It also depends on the cross-linking agent that's used to cure the epoxy, which could take it to the higher end of the temperature range mentioned above.