Problem Solving Forum
October 2 - October 8, 2016
What action should be taken if the IOZ fails the MEK test?
Selected Answers
From
OM PRAKASH JAT of Galadari Engineering works on
December 10, 2016:
Humidity above 70% is required to speed up the cur ...read more
Humidity above 70% is required to speed up the curing process. If such high humidity is not possible, then you must sprinkle water on the substrate for IOZ to cure properly.
From
Per Gabrielsson of Free Lance Consultations and Inspections on
October 7, 2016:
I mean, if the MEK test fails after a week, there ...read more
I mean, if the MEK test fails after a week, there is no guarantee of a full hydrolysing, and, thus, a full reblasting is required.
From
Per Gabrielsson of Free Lance Consultations and Inspections on
October 4, 2016:
Conduct a full reblast and reapplication. ...read more
Conduct a full reblast and reapplication.
From
Kiran Pawar of Asiab Paints Berger Bahrain on
October 4, 2016:
In this case, you have to sprinkle water to accel ...read more
In this case, you have to sprinkle water to accelerate the curing.