What are the most important recommendations for successful field application of reflective coatings to aging single-ply roofs?
Selected Answers
From
Tim Davis of J3 Systems on
September 28, 2016:
Do not present the coating as a "miracle in a buck ...read more
Do not present the coating as a "miracle in a bucket" to the client. Conduct an EC or infrared scan of the roof for trapped moisture.
Prep, prep, prep your details, flashings and penetrations.