Which type of abrasive blasting media is suitable for preparing the more “exotic” stainless steels, such as Inconel or Monel?


Selected Answers

From Giuseppe Santagata of NACE Certif. Coat. Insp. level III # 2737 on April 8, 2014:
Most suitable are corundum, garnet and olivine. ...read more

From Ron Ward of Environmental Abrasives Warehouse on March 17, 2014:
Garnet or crushed glass ...read more