What’s the best way to protect porous masonry from graffiti?
Selected Answers
From
Brian Hall of Brichem Sales Ltd. on
January 3, 2014:
The most effective and least costly graffiti prote ...read more
The most effective and least costly graffiti protection over the long haul is by using polysiloxane (silicone technology) coatings that come in clear or in a rainbow of colors, will last for 10+ years and will allow over 95% of all spray paint graffiti to be washed off with plain cold water.