What is the best way to protect an exposed concrete foundation?


Selected Answers

From KARL BRINKMANN of PURE ASPHALT on November 27, 2013:
Try using a gray polymer rubber emulsion waterproo ...read more

From Pete Salmon of Perkins+Will on November 25, 2013:
Apply an elastomeric coating, as it provides water ...read more