Where there is likely to be ponding water, what generic type of reflective roof coating will work best and why?
Selected Answers
From
Joe Spagnolo of Sealoflex on
October 31, 2022:
Dark gray silicone on roofs.
It’s resistant to p ...read more
Dark gray silicone on roofs.
It’s resistant to ponding water and heats up enough to help in evaporation.