What is the best and quickest method for removing a polyurea tank lining?
Selected Answers
From
palanisamy moovarsan of TECHNIP on
August 14, 2021:
The best and quickest method for removing a polyur ...read more
The best and quickest method for removing a polyurea tank lining is ordinary dry abrasive blast and coated.
From
Mike Makela of Sunstate Coatings Inc. on
August 12, 2021:
UHP blasting 40k ...read more
UHP blasting 40k
From
mauricio gomez of Jifco inc on
August 12, 2021:
Removing Elastomeric coatings, and linings my best ...read more
Removing Elastomeric coatings, and linings my best experience removing that is using a heather torch and scrape with putty knife.
From
Dudley Primeaux of Primeaux Associates LLC on
August 11, 2021:
If it is an elastomeric polyurea system, that has ...read more
If it is an elastomeric polyurea system, that has been properly applied to a properly prepared substrate, the best and fastest method of removal is via High Pressure Water Jetting. And depending upon applied film thickness of the polyurea, may require Ultra-High Pressure Water Jetting.
From
Gordon Kuljian of GK Consulting LLC on
August 10, 2021:
Hands down UHPWJ with rotating tip and cutting jew ...read more
Hands down UHPWJ with rotating tip and cutting jewels. You will have to deal with the waste-water and waste coating.
GK