When performing maintenance painting of tank coatings, what are the pros and cons of overcoating an existing lining that appears to be in good condition?


Selected Answers

From Jaime Marcos of Profesional independiente on September 15, 2020:
Pros: Execution period (entry into service in a short time). Reduced cost. Valid for tanks with little responsibility. Cons: There may be undetected areas with poor adherence. The detachment of the paint layer, in addition to corrosion, can lead to load contamination. Corrosion spots that have not come to the surface of the coating. Other faults in the coating not visible to the naked eye. The quality of the coating cannot be assured. If the contents of the tank are responsible, the interior lining must be done completely again (blast cleaning and application of the paint system).

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; Coating Application; EMEA (Europe, Middle East and Africa); Latin America; Linings; North America


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
KTA-Tator, Inc. - Corporate Office

 
DeFelsko Corporation

 
SAFE Systems, Inc.

 
Strategic Materials Inc.

 
WEFTEC Show

 
Sauereisen, Inc.

 
Tarps manufacturing, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us