What types of measures can be taken on or around metal pipes or columns that penetrate concrete or asphalt paving to reduce corrosion at the interface?


Selected Answers

From Wayne Senick of Termarust Technologies on August 25, 2020:
Most standard barrier systems micro-crack and have no activity, especially the ability to neutralize acid. A solution we have seen in the field is to use a chemically active alkaline coating (acid neutralizer) near the interface and then cover the wet coating with tar paper if immediate back-fill is required to protect the coating from the dirt, concrete or asphalt. Cheap and quick but addresses the problem with the right chemistry.

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; Corrosion; EMEA (Europe, Middle East and Africa); Good Technical Practice; Latin America; North America


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
HoldTight Solutions Inc.

 
Sauereisen, Inc.

 
NLB Corporation

 
Paint BidTracker

 
Modern Safety Techniques

 
Strand’s Industrial Coatings

 
Tarps manufacturing, Inc.

 
CRW

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us