How do you measure the DFT or WFT of a film-forming sealer applied to a metallized coating (e.g., flame-sprayed zinc)?


Selected Answers

From Janssen Christophe of Lassarat on August 26, 2020:
As said before, the layer must not be a fully closed paint film. A light quantity of paint is sufficient. The only reason to apply this is to seal the porosity of the TSA and avoid popping when applying the overcoat.

From Jaime Marcos of Profesional independiente on August 17, 2020:
As it is about sealing the porosity of the surface, it is enough to cover the entire surface. (It is usually said, "layer at zero microns.") It is not necessary to measure the thickness of the paint layer. It is enough that the entire surface is covered, since its function is not barrier layer proportions.

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; Coating Application; EMEA (Europe, Middle East and Africa); Latin America; Metallizing; North America


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
KTA-Tator, Inc. - Corporate Office

 
DeFelsko Corporation

 
SAFE Systems, Inc.

 
Sauereisen, Inc.

 
WEFTEC Show

 
Strategic Materials Inc.

 
Tarps manufacturing, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us