I’ve heard about using crystalline admixture or crystalline materials on top of concrete to fill voids and make the substrate less permeable. When is this desirable, and what is the best way to use these materials?


Selected Answers

From Bart Bergsbaken of SPG on May 11, 2020:
Crystalline admixtures are reactive to moisture movement. There are proactive solutions that do not affect materials from bonding to the concrete.

Please sign in to submit your answer this question    

Tagged categories: Asia Pacific; EMEA (Europe, Middle East and Africa); Latin America; Maintenance + Renovation; North America; Permeability


Current PSF Question | Submit a PSF Question | Full PSF Archive

Advertisements
 
WEFTEC Show

 
DeFelsko Corporation

 
Sauereisen, Inc.

 
SAFE Systems, Inc.

 
Tarps manufacturing, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us